Investigation of metallurgical and mechanical properties of TIG welded parts for material replacement

Authors

Abstract

In this research, metallurgical and mechanical properties of TIG welded parts were investigated. For this purpose, TIG welding operation with optimum input parameters was carried out on XH50 and Hastelloy x rolled sheets. For comparison these two materials and feasibility of material replacement, initially elemental analysis of the two materials was accomplished and then the properties such as microstructure, tensile strength and micro-hardness were examined for both initial and welded specimens. The results show that heat affected zone in Hastelloy x welded samples is wider than XH50 welded samples and Heat affected zone in Hastelloy x welded samples consists of three regions. Despite the same tensile properties of the two materials, micro-hardness of the initial material and also tensile strength and micro-hardness of the welded specimen for Hastelloy x were significantly higher than XH50. The average of tensile strength for Hastelloy x welded samples is approximately 31% higher than that for XH50 welded samples due to formation brittle phases in XH50 samples. Therefor Hastelloy x is more desirable than XH50 for TIG welded parts.

Keywords

Main Subjects


[1]  Rack ML (1998) Titanium alloys in total joint replacement—a materials science perspective. Biomaterials 19(18):1621-1639.
[2]  Sibly TF,  Unsworth A (1991)  Wear of cross-linked polyethylene against itself: a material suitable for surface replacement of the finger joint. J Biomed Eng 13(3): 217-220.
[3]  Fagan MJ (1986) Material selection in the design of the femoral component of cemented total hip replacements. Clin Mater  1(3): 151-167.
[4]  El-Sheikh HF, Mac Donald BJ , Hashmi MSJ (2002) Material selection in the design of the femoral component of cemented total hip replacement. J Mater Process Technol 122(2-3): 309-317.
[5]  Taksali S,  Grauer JN, A. Vaccaro R (2004) Material considerations for intervertebral disc replacement implants. The Spine J 4(6): 231-238.
[6]  Katti KS (2004) Biomaterials in total joint replacement. Colloids Surf B: Biointerfaces  39(3): 133-142.
[7]  Bahraminasab M, Jahan A (2011) Material selection for femoral component of total knee replacement using comprehensive VIKOR. Mater & Des 32(8–9): 4471-4477.
[8]  Fallahnezhad K,  Farhoudi H,  Oskouei R H,  Taylor M (2016) Influence of geometry and materials on the axial and torsional strength of the head–neck taper junction in modular hip replacements: A finite element study. J Mech Behav Biomed Mater  60:118-126.
[9]  Rubel H,  Marschke D,  Tautz J,  Micheel G (1989) Inconel X-750 as material for core internals and core components - Status of in-service experience and replacements at siemens kwu group. Nucl Eng Des 112: 329-336.
[10] Anwar R , Vermol VV, Rahman S, Hassan OHR  , Dung TW (2014) Reformulating Local Ceramic Stoneware with Alumina as Replacement Material for the Heat Sink. JAH 31: 507-516.
[11] Groover MP (2010) Fundamentals of modern manufacturing: materials, processes and systems. 4rd edn., Wiley, New York.
[12] Huang B, Zhang J, Wu Q (2017) Microstructure and mechanical properties of China low activation martensitic steel joint by TIG multi-pass welding with a new filler wire. Nucl Mater 490: 115-124.
[13] Vidyarthy RS, Kulkarni A, Dwivedi DK (2017) Study of microstructure and mechanical property relationships of A-TIG welded P91–316L dissimilar steel joint. Mater Sci Eng A 695: 249-257.
[14] Wang G, Li Q, Li YJ, Wu AP, Ma NX, Yan DY, Wu HQ (2017) Effects of weld reinforcement on tensile behavior and mechanical properties of 2219-T87 aluminum alloy TIG welded joints. TNMSC 27: 10-16.
[15] Donachi MJ, Donachi SJ (2002) Superalloys a technical guide. 2re edn., ASM International, Materials Park, Ohio.
[16] Bradly EF (1998) A technical guide of superalloys. ASM International, Materials Park, Ohio.
[17] Charre MD (1997) The microstructure of superalloys. Clima Molybdenium Co. Sym., Zurikh.
[18] Marriott JB, Merz M, Nihoul J, Ward IM (1987) High temperature alloys, Springer, New York.
[19] Betteridge W, Shaw SWK (1987) Development of superalloys. Mater sci technol 3(9): 682-694.
[20] Decker RF, Smits CT (1972) The Metallurgy of nickel base superalloys. Paul D. Merica Research laboratory, New York.
[21] Smits CT (1984) A history of superalloy metallurgy for superalloy metallurgist. The metallurgical society of AIME, Warrendale.
[22] Villars P, Prince A, Okamoto H (1995) Handbook of ternary alloy phase diagrams, ASM International, Materials Park, Ohio.
[23] Zhang Li, Gobbi SL, Richter KH (1997) Autegenous welding of Hastelloy X to MAR-M247 by laser. J Mater Process Technol 70:285-292.